Korrosionsbeständigkeit | Ausgezeichnet. |
---|---|
Reinheit | 99.95% |
Chemische Resistenz | Hoch |
Wärmeleitfähigkeit | 105 W/mK |
Anwendungen | Schmelztiegel, Feuerfeste, Gießereibeschichtungen |
Corrosion Resistance | Excellent |
---|---|
Purity | 99.95% |
Chemical Resistance | High |
Thermal Conductivity | 105 W/mK |
Applications | Crucibles, Refractories, Foundry Coatings |
Corrosion Resistance | Excellent |
---|---|
Purity | 99.95% |
Chemical Resistance | High |
Thermal Conductivity | 105 W/mK |
Applications | Crucibles, Refractories, Foundry Coatings |
Corrosion Resistance | Excellent |
---|---|
Purity | 99.95% |
Chemical Resistance | High |
Thermal Conductivity | 105 W/mK |
Applications | Crucibles, Refractories, Foundry Coatings |
Corrosion Resistance | Excellent |
---|---|
Purity | 99.95% |
Chemical Resistance | High |
Thermal Conductivity | 105 W/mK |
Applications | Crucibles, Refractories, Foundry Coatings |
Wärmeleitfähigkeit | 110 bis 125 W/mK |
---|---|
Porosität | 12-15% |
Flexuralstärke | Mpa 60 |
Der Wärmeausdehnungskoeffizient | 5.2 x 10^-6 /K |
Dichte | 10,85 g/cm3 |
Druckfestigkeit | 175 Mpa |
---|---|
Härte | 65 HS |
Dichte | 20,72 g/cm3 |
Farbe | Metallisches Grau |
Material | Kupfer und Graphit |
Wärmeleitfähigkeit | 130 W/m·K |
---|---|
Korrosionsbeständigkeit | Ausgezeichnet. |
Farbe | Schwarz |
Koeffizient der thermischen Ausdehnung | 4.8 x 10^-6 /K |
Dichte | 10,7 g/cm3 |
Massendichte | 10,71 g/cm3 |
---|---|
Druckfestigkeit | mpa 30 |
Flexuralstärke | Mpa 15 |
elektrischer Widerstand | 9 bis 10 μΩ.m |
Shorehärte | 30 HSD |
Corrosion Resistance | Excellent |
---|---|
Purity | 99.95% |
Chemical Resistance | High |
Thermal Conductivity | 105 W/mK |
Applications | Crucibles, Refractories, Foundry Coatings |